316 tiub keluli tahan karattersedia dalam pelbagai saiz untuk memenuhi keperluan yang berbeza dalam industri seperti pemprosesan kimia, minyak dan gas, dan aplikasi marin. Berikut ialah beberapa saiz dan spesifikasi standard:
Dimensi Saiz Tiub Keluli Tahan Karat 316
| Diameter Luar (OD) | Ketebalan Dinding (WT) | Diameter Dalam (ID) |
|---|---|---|
| 1/8" (3.18 mm) | {{0}}.035" (0.89 mm) | 0.115" (2.92 mm) |
| 1/4" (6.35 mm) | {{0}}.035" (0.89 mm) | 0.215" (5.46 mm) |
| 1/4" (6.35 mm) | 0.049" (1.24 mm) | 0.203" (5.16 mm) |
| 3/8" (9.53 mm) | {{0}}.035" (0.89 mm) | 0.305" (7.75 mm) |
| 3/8" (9.53 mm) | 0.049" (1.24 mm) | 0.283" (7.19 mm) |
| 1/2" (12.7 mm) | {{0}}.035" (0.89 mm) | 0.430" (10.92 mm) |
| 1/2" (12.7 mm) | 0.049" (1.24 mm) | 0.402" (10.21 mm) |
| 1/2" (12.7 mm) | 0.065" (1.65 mm) | 0.370" (9.40 mm) |
| 3/4" (19.05 mm) | 0.049" (1.24 mm) | 0.652" (16.56 mm) |
| 3/4" (19.05 mm) | 0.065" (1.65 mm) | 0.620" (15.75 mm) |
| 1" (25.4 mm) | 0.049" (1.24 mm) | 0.902" (22.91 mm) |
| 1" (25.4 mm) | 0.065" (1.65 mm) | 0.870" (22.10 mm) |
| 1" (25.4 mm) | 0.083" (2.11 mm) | 0.834" (21.18 mm) |
| 1-1/4" (31.75 mm) | 0.065" (1.65 mm) | 1.120" (28.45 mm) |
| 1-1/4" (31.75 mm) | 0.083" (2.11 mm) | 1.084" (27.53 mm) |
| 1-1/2" (38.1 mm) | 0.065" (1.65 mm) | 1.370" (34.80 mm) |
| 1-1/2" (38.1 mm) | 0.083" (2.11 mm) | 1.334" (33.88 mm) |
| 2" (50.8 mm) | 0.065" (1.65 mm) | 1.870" (47.50 mm) |
| 2" (50.8 mm) | 0.083" (2.11 mm) | 1.834" (46.58 mm) |
| 2" (50.8 mm) | 0.095" (2.41 mm) | 1.810" (45.97 mm) |
| 2-1/2" (63.5 mm) | 0.083" (2.11 mm) | 2.334" (59.29 mm) |
| 2-1/2" (63.5 mm) | 0.095" (2.41 mm) | 2.310" (58.67 mm) |
| 3" (76.2 mm) | 0.083" (2.11 mm) | 2.834" (71.98 mm) |
| 3" (76.2 mm) | 0.095" (2.41 mm) | 2.810" (71.37 mm) |
| 4" (101.6 mm) | 0.083" (2.11 mm) | 3.834" (97.42 mm) |
| 4" (101.6 mm) | 0.095" (2.41 mm) | 3.810" (96.82 mm) |
| 6" (152.4 mm) | 0.109" (2.77 mm) | 5.782" (146.85 mm) |
316 Saiz Tiub Keluli Tahan Karat Diameter Luar (OD)
- Tiub Bor Kecil: 1/16" hingga 1/2" (1.59mm hingga 12.7mm)
- Tiub Bor Sederhana: 5/8" hingga 1" (15.88mm hingga 25.4mm)
- Tiub Bor Besar: 1 1/4" hingga 2" (31.75mm hingga 50.8mm)
- Tiub Bore Lebih Besar: 2 1/4" hingga 4" (57.15mm hingga 101.6mm)
Saiz Tiub Keluli Tahan Karat 316 Ketebalan Dinding
- Dinding Nipis: {{0}}.028" hingga 0.065" (0.71mm hingga 1.65mm)
- Dinding Standard: {{0}}.083" hingga 0.12" (2.11mm hingga 3.05mm)
- Dinding Berat: {{0}}.156" hingga 0.25" (3.96mm hingga 6.35mm)
ss 316 Saiz Tiub Panjang
- Panjang Standard: 20 kaki (6.096 meter)