347 Stainless Steel Plate

347 Stainless Steel Plate


1. Standard: ASTM A240 / ASME SA240 / AMS5512
2. Width: 0~2500mm or as per your requirements
3. Length: 0~12m or as per your requirements
4. Thickness: 0.3~1200mm or as per your requirements
5. Grades:AISI 347,UNS S34700, EN 1.4550
Hantar pertanyaan
pengenalan produk

347 Stainless Steel Plate is a niobium stabilized austenitic stainless steel plate. SS 347 Plate has excellent resistance to intergranular corrosion when exposed to the chromium carbide precipitation temperature range of 800 – 1500 degree F (427 – 816 degree ). Alloy 347 has good oxidation resistance and creep strength up to 1500 degree F (816 degree ). The corrosion resistance of annealed 347 alloy is stronger than that of 321 alloy in the annealed condition in strongly oxidizing environments.

 

ASTM A240 347 Stainless Plate Standard:

  • ASTM A240: Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

 

  • : HT PIPE is a leading supplier and exporter of ASTM A240 347 steel plate. We have passed ISO9001:2000 and API quality certification system qualifications, and we provide products in different sizes, thicknesses and shapes.
347 stainless steel plate

ASTM A240 UNS S34700 Plate Specification 

ASTM A240 / ASME SA240 Stainless Steel Plates
304, 304L, 310S, 310, 316, 316L, 316Ti, 317, 317L, 321, 321H, 347, 347H,904L, 254 SMO, Duplex, etc
Cold rolled: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm or as your requirement.
Hot rolled: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm or as your requiremnt.
2B, 2D, BA, NO. 1, NO. 4, NO.8, 8K, Mirror, Checkered, Embossed, Hair Line, Sand Blast, Brush, Etching

 

1.4550 Stainless Steel Plate Chemical Composition

ASTM A240M Chemical Composition
C P S
SUS347 Less than or equal to 0.08 Less than or equal to 0.75 Less than or equal to 2.00 Less than or equal to 0.045 Less than or equal to 0.030 9.0-13.0 17.0-19.0 ― Nb:10C/1.00

 

Alloy 347 Stainless Steel Plate

SUS347 Greater than or equal to 205 Greater than or equal to 515 Greater than or equal to 40 Less than or equal to 201 Less than or equal to 92

 

SUS 347 Stainless Steel Properties Acid Corrosion Resistance

ASTM A240 UNS S34700 Plate can be used in most dilute organic acids at moderate temperatures and pure phosphoric acid at lower temperatures and up to 10% dilute solutions at elevated temperatures. WNR 1.4550 Stainless Steel Plate resists polysulfuric acid stress corrosion cracking in hydrocarbon service.

 

Application of ASME SA240 UNS S34700 Plate

  • Heat Exchangers: Heat Exchangers and High-Temperature Furnace Shells, etc.
  • Petroleum Refining - Fluidized Catalytic Cracking Units, Polythionic Acid Services.

 

 

Q: About 347 Stainless Steel Plate price per kg?

A: Prices ranges from $5 to $10 per kg.

A: Delivery time is within 5-21 days

Q: How to pack the SA240 S34700 products?

 

 

Cool tags: 347 stainless steel plate, 347 plate, 347 stainless plate